Goliath hotend, VZhextrudort extruder, .4 standard nozzle.
305C ABS(that's what it wanted, so that's what I gave it)
600mms, 30K acceleration, 30SCV internal, external wall 12KA, 20SCV.
.015PA, 50% CPAP fan all but bridges @20% cooling.

Annex cube, 175%, sunk into the build plate so I can get to the bridge quicker and test rest of model without printing the whole thing.

Working on a quality profile and trying to get more out of Super Slicer.

I was playing with bridging and my CHT is not doing good bridges! Changed to .4 standard and all is well. Fouled CHT? Or back-pressure causing curl?

Bridges seemed to work well at 150-200mms @ 15K acceleration, 60-70% density ,100% flow, and 20-30% fan. Still a work in progress.

Top skin I tried to do 45° and it didn't turn out so well for this model. I had also increased line density for top skin, which was a mistake. The joys of tuning.

Wondered why my infill flow was so high when the rest of the print, same speed, had less flow.. That "combine infill every X layers" got me! Perhaps I can do it again with combine at 1 and reduce the # of top layers.

Always something.. Make no mistake, this print is solid and not much fan needed!