Uploaded September 2016 | Updated November 2026, 18 hours ago
Warning:
Do absolutely not try this experiment! We tried it for several times now and the acid never completely destroyed the glass even after days. Still glasses vary and acid conc. may as well change. In comparison with other demonstrations on the net it seems like this reaction can be really violent. So it can't be predicted how it will react with your glass. Absolutely do not do this. HF is highly toxic and can penetrate the skin in a short time!
This is what happens if Hydrofluoric Acid (40%) is added to a glass test tube. It reacts very fast causing a sudden blur on the glass. We tried this at cold temperatures and below 0°C nothing really happens even after some days. At warmer temperatures around 30°C (this video) it reacts very fast. It doesn't eat all the way through the glass in seconds (even in larger batches) but is incredibly fast. If higher conc. are used the temperature becomes so hot that it catalyzes the reaction and in these cases it may it eat through the glass in a short time causing the acid to spill on the table.
------------------------------------------------------------------
Second part of this video was the question whether it would smoke the same way forming NH4F like HCl does if NH4OH is added. So we added some Ammonia to it and it started to fume in a similar way.
------------------------------------------------------------------------------------------
Still we should take some time to explain why HF attacks glass. This explanation will follow soon !
Warning:
Do absolutely not try this experiment! We tried it for several times now and the acid never completely destroyed the glass even after days. Still glasses vary and acid conc. may as well change. In comparison with other demonstrations on the net it seems like this reaction can be really violent. So it can't be predicted how it will react with your glass. Absolutely do not do this. HF is highly toxic and can penetrate the skin in a short time!
This is what happens if Hydrofluoric Acid (40%) is added to a glass test tube. It reacts very fast causing a sudden blur on the glass. We tried this at cold temperatures and below 0°C nothing really happens even after some days. At warmer temperatures around 30°C (this video) it reacts very fast. It doesn't eat all the way through the glass in seconds (even in larger batches) but is incredibly fast. If higher conc. are used the temperature becomes so hot that it catalyzes the reaction and in these cases it may it eat through the glass in a short time causing the acid to spill on the table.
------------------------------------------------------------------
Second part of this video was the question whether it would smoke the same way forming NH4F like HCl does if NH4OH is added. So we added some Ammonia to it and it started to fume in a similar way.
------------------------------------------------------------------------------------------
Still we should take some time to explain why HF attacks glass. This explanation will follow soon !

 is formed in dilute, cold KOH which is further reduced to the orange [RuO4](2-) containing Ru(VI) if the conc. Is raised.
So much like with Cyanide, Ruthenium will undergo a redox reaction with the reactant before forming the new compound.
To the right glass we added some Hydrochloric acid. It quickly turned orange and over some time to a dark orange-red. This is due to two possible species that form under these conditions:
A [RuO2Cl4](2-) containing Ru(VI) and the Ru(IV) compound [Ru2OCl10](4-). The latter one contains two [RuCl5]-octahedra which are connected via an oxygen as their sixth ligand. Many other acids and compounds react in a similar way which is why all the solutions you saw (the yellow RuO4 solutions we boiled) turned dark red after a few days.
We think this last part showed that in fact we made some Ru(VIII) as in all other experiments where we used HCl (and those were a lot, although most never made it to YouTube) it would never change to this colour and only Ru(VIII) is said to behave like this.
The second thing is, usually we search for these experiments in old analytical chemistry books. But for the platinum group metals there isn’t much information. In fact, go look for some Ruthenium chemistry and see what you can find. It took us quite some amount of effort, looking at our University’s library for very old books on the subject, a special book about Ruthenium chemistry which is about 1400 pages long and many more extra books. For a long time we were unsure whether our reactant might be contaminated, which couldn’t be as we recently bought it for these experiments or the books were wrong. Which is why sometimes we had to test them out in very different ways and compare the results in the end. This however seems to be a very useful way to test for Ruthenium, to heat it in a dilute acid with some oxidizers and test the gas with dilute HCl. Be careful when doing this other compounds might not like being heated with permanganate for example. Do this if you are really sure your compound is ruthenium based! Ruthenium Chemistry: Some chemistry with RuO4](https://i.ytimg.com/vi/GN85s88if4Y/mqdefault.jpg)




In this video we are looking back at CuCN, the compound that forms when Cu(CN)2 gets reduced by Cyanides. While being insoluble it can be brought back into solution by adding more Cyanide to it forming [Cu(CN)4](3-).
This time however we add Thiocyanate which is also a Pseudo-Halogen to it forming the soluble [Cu(CN)3(SCN)](3-).
Many Cyanides can be good precursors for other compounds and although they are strong ligands sometimes they can easily be knocked off. Copper Chemistry: [Cu(CN)3(SCN)](3-)](https://i.ytimg.com/vi/HzTh_S5lZ00/mqdefault.jpg)


![K3[V(CN)5NO] (???)
Well...to be honest we do not know what this is either!
Much like Sodium Nitroprusside other elements form Pentacyano-Nitrosyl-Metallates, too. For this often, Hydroxylamine is used together with Cyanide on the metal solution.
We found a text saying that Vanadium(V) would react with Hydroxylamine and KCN at 100°C to form an orange compound. As we only had Hydroxylamine-Hydrochloride we still gave it a chance.
Ammoniummetavanadate, KCN and Hydroxylamine-Hydrochloride were dissolved in water and boiled for some seconds. The colour changed to an orange as mentioned in the literature and a brown gas is liberated, probably Nitrous Oxides.
The problem with these type of compounds are that all of them were collected in books around the same time and have been copied since then. Today we know for example that the brown ring test contains no Iron(I) but Iron(III) and a NO(+). The same thing applies for those Pentacyanonitrosyl-Metallates. Many books automatically assume they have to be in an oxidation state +1.
This Vanadium compound was originally published to be V(-1), yes a stable -1 Metal but newer studies show it’s in fact a K3[V(CN)5(NO)]. We think many of these compounds have to be checked again, which is why we usually do not mention them. This is an exception as there is not much Vanadium chemistry you can easily do and this reaction worked so well.
We tried it again with Cyanide and Vanadate only and it would not change colours! K3[V(CN)5NO] (???)](https://i.ytimg.com/vi/IVpv_x22QAE/mqdefault.jpg)

![Phosphorus Chemistry: PBr5 formation
In this video we will try to make Phosphorus Bromides. As we dont want to isolate elemental Bromine for this reaction we thought of making a tiny amount in a test tube and use the vapors in the upper half of the tube as our source of pure bromine. Therefore we added some red Phosphorus to the tip of a glass pipette and hung it in the vapors.
Part one of the video is the synthesis of Bromine. Potassium Bromide is placed in a test tube and 3% Hydrogen Peroxide is added. To this conc. Sulfuric Acid is dropped. Now many say the Acid will displace HBr which is oxidized by Peroxide but I try to stay closer to the actual redox reaction.
H2O2 + 2 H3O(+) + 2 e(-) to 4 H2O
As you can see H3O(+) or H(+) if you shorten the equation is required to compensate the extra Oxides. These redox reactions, much like the Chromate and Permanganate redox reactions depend on pH values. And a bit of acid is required to reach this high redox potential which allows Bromides to be oxidized to Bromine. Using conc. H2SO4 alone would work as well since it is quite oxidizing and does a similar effect. Here I use the conc. acid since the heat of dilution with the 97% water of the peroxide will heat the mixture up and Bromine starts to boil off.
The second part of the reaction is the Bromination:
First 2 P + 3 Br2 form 2 PBr3 this is liquid and the formation is really exothermic which causes the phosphorus to ignite in the first try. So we probably formed a lot of Oxides as well in this process.
If PBr3 is the desired product an excess of Phosphorus is required to make sure it wont be further brominated. PBr3 can then react with an additional Br2 to form PBr5 which is a solid compound and probably the yellow stuff you can see at the end in the pipette. PBr5 has a quite interesting structure as one would suspect a trigonal bipyramid with a serious Berry-Pseudo Rotation it actually forms [PBr4][Br] structures which can be formulated as Bond-No-Bond-structures much like Polyiodides have them.
Upon further reaction compound like PBr7 might form as well. Those will have Polybromides to avoid a too high coordination on the Phosphorus.
What you can see is first the formation of Bromine vapors, then the reaction and ignition of Phosphorus with Bromine and later some red Phosphorus in an Bromine atmosphere which will upon reaction slowly discolor the gas phase as the Bromine is consumed by the reaction. Phosphorus Chemistry: PBr5 formation](https://i.ytimg.com/vi/J6Xj_lEbj9M/mqdefault.jpg)