Uploaded May 2021 | Updated September 2026, 2 hours ago
cast an aluminum plaque with the intention of anodizing and dyeing it. This was my first attempt at anodization and well... I can stand to learn a few things.
Here's Mark's video youtu.be/Z1zT8p7d9Z0
Visit me on Instagram at instagram.com/realswdweeb
My models are now available on my online store at plmfoundries.com/shop
I get asked about the moisture content of my sand. I have settled on a ratio of about 2 liters of sand and 36-42ish ml of water for my ratio. I start with sand that is dry.
#beablessing #metalcasting #notcovidrelated
cast an aluminum plaque with the intention of anodizing and dyeing it. This was my first attempt at anodization and well... I can stand to learn a few things.
Here's Mark's video youtu.be/Z1zT8p7d9Z0
Visit me on Instagram at instagram.com/realswdweeb
My models are now available on my online store at plmfoundries.com/shop
I get asked about the moisture content of my sand. I have settled on a ratio of about 2 liters of sand and 36-42ish ml of water for my ratio. I start with sand that is dry.
#beablessing #metalcasting #notcovidrelated