apocalypsehighway | Review: Pt.2 USC All Metal Mixing/Application @apocalypsehighway | Uploaded 10 years ago | Updated 3 hours ago
Here I show you, the easy mix and application of
USC All Metal Body Filler..
This is the best for repairing/covering metal work/welding or other such blemishes that Bondo just is not good for.
Remember.. this is metal, repairing metal.
Mixing tips: 12 to 15 drops *use a thumbtack or safety pin to make the hole* and I do mean drops of the catalyst into/onto the potato sized pile of All Metal is all that is needed. IF you use too, little it will flake off or fall in chunks off the applied area during it's sanding (Pt.3 Pt.3 http://www.youtube.com/watch?v=vbKFr9lMFTk) process.
Here I show you, the easy mix and application of
USC All Metal Body Filler..
This is the best for repairing/covering metal work/welding or other such blemishes that Bondo just is not good for.
Remember.. this is metal, repairing metal.
Mixing tips: 12 to 15 drops *use a thumbtack or safety pin to make the hole* and I do mean drops of the catalyst into/onto the potato sized pile of All Metal is all that is needed. IF you use too, little it will flake off or fall in chunks off the applied area during it's sanding (Pt.3 Pt.3 http://www.youtube.com/watch?v=vbKFr9lMFTk) process.