Commercial casting slips are great for their convenience, but what do you do when your recipe hard-pans in the bucket? Today the gang talk about why hard-panning happens and how you can fix it. They also discuss making temp checks, the best bisque temp for commercial glazes, and the controversy around the sale of fake ceramic pigments.

Do you have questions or need advice on glazes?
➤ Drop us a line at ForFluxSakePodcast@gmail.com and you could be featured on an upcoming show.

Have you checked out the new For Flux Sake Patreon? This is a great way to show your support and have access to discounted merch, live hangouts, and extra episodes. Head over to Patreon (patreon.com/c/ForFluxSakePodcast/) OR (Link in bio!) and sign up today.

🎙️Today’s episode is brought to you by:
Monkey Stuff (monkeystuff.com/)
The Rosenfield Collection (rosenfieldcollection.com/)
Cornell Studio Supply (cornellstudiosupply.com/)
Making Glazes, Make Sense (ceramicmaterialsworkshop.com/courses/making-glazes-make-sense.html)

For Flux Sake is hosted by Matt and Rose Katz of the Ceramics Materials Workshop along with Kathy King ( @kathykingart ) of the Harvard Ceramics Program. Together they answer your burning questions about clay and glaze. In each episode they answer listener submitted questions in a comical, but also insightful way. This show will have you laughing and learning about glaze chemistry the chemistry behind ceramics in no time. New episodes typically drop every 2 weeks.

⭐️WE GOT A NEW ARTIST! Everyone give much needed love to Jenny ( @jennyblicharzceramics ) who made this graphic (and is also a stellar ceramicist) and will now be working with us to make some more killer graphics!

#Materialscorner #hardpanning #castingslip #commercialglaze #tempchecks #ceramicpodcast #podcast
Why is my casting slip hard-panning? | For Flux Sake Episode 117Clay Body Profiling Livestream pt. 1 | Ceramic Materials WorkshopGlaze is glass! | Ceramic Materials WorkshopDo You NEED Titanium?! | Ceramic Materials WorkshopCeramic Consulting: Solutions and Support | Ceramic Materials WorkshopBristol Glazes - Limitations and Color Dynamics Explained | Ceramic Materials WorkshopHave you used a Dilatometer before? | Ceramic Materials WorkshopBest Clay Bodies for Accurate Results | Ceramic Materials WorkshopGabriel Kline and Bill Collins on food safe glazes | For Flux Sake 119Dunting - Glaze Chemistry | Ceramic Materials WorkshopDo I really need to sieve my glazes? | For Flux Sake 123Descifrando el Horno | Cómo funcionan los esmaltes Bristol | Ceramic Materials Workshop
Ceramic Materials Workshop |

Why is my casting slip hard-panning? | For Flux Sake Episode 117

SHARE TO X SHARE TO REDDIT SHARE TO FACEBOOK WALLPAPER