Uploaded June 2020 | Updated November 2026, 6 hours ago
Our crew is putting back 6 iron rings on the main mast. The rings are heated up to 800 degrees and are placed on the mast. Once the rings are in place they are cooled with water so that the metal shrinks and it will keep the pieces of the mast together!
Our crew is putting back 6 iron rings on the main mast. The rings are heated up to 800 degrees and are placed on the mast. Once the rings are in place they are cooled with water so that the metal shrinks and it will keep the pieces of the mast together!