Uploaded February 2026 | Updated November 2026, 6 hours ago
Learn how to tumble obsidian in a rotary rock tumbler without cloudy haze, chipped edges, bruising or deep scratches. This complete obsidian tumbling tutorial shows the four-stage process I used to turn rough Flagstaff-area volcanic glass into a deep black mirror finish.
Obsidian can be more difficult to tumble than agate or jasper because it is brittle and easily damaged. A barrel that is too aggressive, insufficient cushioning, trapped grit or one damaged stone can affect the entire batch.
In this video, you’ll see:
• How full to keep the rotary tumbler barrel
• How to cushion brittle obsidian during tumbling
• When to add ceramic tumbling media
• How to inspect and sort the stones between stages
• Why chips, pits and fractures should not advance
• How grit contamination causes deep scratches
• How to use aluminum oxide pre-polish and polish
• How to remove polish residue with a final burnishing cycle
• What properly polished obsidian should look like when completely dry
The complete obsidian tumbling process:
Stage 1 — 60/90 silicon carbide coarse grit
Stage 2 — 150/220 silicon carbide medium grit
Stage 3 — 500 aluminum oxide pre-polish
Stage 4 — High-quality aluminum oxide polish
Final cleanup — Dawn dish soap and water burnish
The most important lesson is not to advance the obsidian automatically just because seven days have passed. Treat every stage as an inspection point. Repeat the stage when you still see chips, pits, fractures or scratches.
Clean the rocks, barrel, lid, seal and tumbling media thoroughly between every stage. For the final polish, dedicated clean ceramic media can reduce the chance of carrying older grit into the barrel.
Never pour rock-tumbling slurry into household plumbing.
CHAPTERS
00:00 Rough obsidian to mirror finish
00:54 Why obsidian is difficult to tumble
01:45 The four-stage tumbling plan
02:05 Stage 1 — 60/90 coarse grit
03:34 Stage 2 — 150/220 medium grit
05:54 Stage 3 — Aluminum oxide pre-polish
08:14 Stage 4 — Final aluminum oxide polish
08:38 The polished obsidian reveal
09:11 Rough versus polished results
What gives you the most trouble when tumbling obsidian: cloudy haze, chipped edges, bruising or scratches?
#Obsidian #RockTumbling #RockPolishing #Lapidary #WillORocks
Learn how to tumble obsidian in a rotary rock tumbler without cloudy haze, chipped edges, bruising or deep scratches. This complete obsidian tumbling tutorial shows the four-stage process I used to turn rough Flagstaff-area volcanic glass into a deep black mirror finish.
Obsidian can be more difficult to tumble than agate or jasper because it is brittle and easily damaged. A barrel that is too aggressive, insufficient cushioning, trapped grit or one damaged stone can affect the entire batch.
In this video, you’ll see:
• How full to keep the rotary tumbler barrel
• How to cushion brittle obsidian during tumbling
• When to add ceramic tumbling media
• How to inspect and sort the stones between stages
• Why chips, pits and fractures should not advance
• How grit contamination causes deep scratches
• How to use aluminum oxide pre-polish and polish
• How to remove polish residue with a final burnishing cycle
• What properly polished obsidian should look like when completely dry
The complete obsidian tumbling process:
Stage 1 — 60/90 silicon carbide coarse grit
Stage 2 — 150/220 silicon carbide medium grit
Stage 3 — 500 aluminum oxide pre-polish
Stage 4 — High-quality aluminum oxide polish
Final cleanup — Dawn dish soap and water burnish
The most important lesson is not to advance the obsidian automatically just because seven days have passed. Treat every stage as an inspection point. Repeat the stage when you still see chips, pits, fractures or scratches.
Clean the rocks, barrel, lid, seal and tumbling media thoroughly between every stage. For the final polish, dedicated clean ceramic media can reduce the chance of carrying older grit into the barrel.
Never pour rock-tumbling slurry into household plumbing.
CHAPTERS
00:00 Rough obsidian to mirror finish
00:54 Why obsidian is difficult to tumble
01:45 The four-stage tumbling plan
02:05 Stage 1 — 60/90 coarse grit
03:34 Stage 2 — 150/220 medium grit
05:54 Stage 3 — Aluminum oxide pre-polish
08:14 Stage 4 — Final aluminum oxide polish
08:38 The polished obsidian reveal
09:11 Rough versus polished results
What gives you the most trouble when tumbling obsidian: cloudy haze, chipped edges, bruising or scratches?
#Obsidian #RockTumbling #RockPolishing #Lapidary #WillORocks










▬▬▬ Watch Next ▬▬▬
▶️ Related Video → https://youtu.be/y2iNLaBFORA
▬▬▬ Chapters ▬▬▬
00:00 – Intro
00:29 – Why Most Rockhounds Fail (Hook)
01:15 – Mistake #1: The Desert Trap
02:33 – Mistake #2: The Aimless Wander
03:51 – Mistake #3: The Gear Gap
05:04 – Mistake #4: Safety Slip-Ups
06:26 – Mistake #5: Lone Wolf Syndrome
07:31 – The Tip That Changed Everything
07:52 – The 5 Mistakes Recap
08:08 – Final Thoughts
#thefinders #arizonarockhounding #rockhoundingtips #lapidarylife 5 Rockhounding Mistakes Everyone Makes in Arizona!](https://i.ytimg.com/vi/RZggNtulsmQ/mqdefault.jpg)