Uploaded August 2021 | Updated September 2026, 7 minutes ago
Casting sprues from the bottom up. The only way to pour 😄
Help keep the videos ad free and purchase many of the items you see in the video at plmfoundries.com
My models are now available on my online store at plmfoundries.com/shop
Visit me on Instagram at instagram.com/realswdweeb
I get asked about the moisture content of my sand. I have settled on a ratio of about 2 liters of sand and 36-42ish ml of water for my ratio. I start with sand that is dry.
#beablessing #metalcasting
Casting sprues from the bottom up. The only way to pour 😄
Help keep the videos ad free and purchase many of the items you see in the video at plmfoundries.com
My models are now available on my online store at plmfoundries.com/shop
Visit me on Instagram at instagram.com/realswdweeb
I get asked about the moisture content of my sand. I have settled on a ratio of about 2 liters of sand and 36-42ish ml of water for my ratio. I start with sand that is dry.
#beablessing #metalcasting